The bottom line
SSPC-PA 2-2022 turns “is the coating thickness acceptable” into a reproducible calculation: it specifies how many areas and spots to measure, how many readings make a spot, and the spot and area limits for acceptance. Follow the procedure and different inspectors should reach the same conclusion.
Document identity
| Item | Content |
|---|---|
| Number | SSPC-PA 2-2022 |
| Document type | Procedure |
| Issuing body | AMPP (formed by the 2021 merger of SSPC and NACE International) |
| Previous editions | Previous revisions: 2015, 2012, 2004, 1996 and 1982; first issued in 1973. |
| Length | The 2022 edition contains 11 appendices; refer to the edition specified by the contract. |
| Companion standard | Must be used together with ASTM D7091-22 |
| Instrument class | Follows the D7091 Type 1 / Type 2 definitions |
Core 1: spot count table
| Coated area | Number of spot measurements |
|---|---|
| ≤ 30 m² (300 ft²) | 5 in every 10 m² (100 ft²) area |
| 30–100 m² (300–1000 ft²) | 15 (5 in each of three 10 m² areas) |
| > 100 m² (1000 ft²): first 100 m² | 15 (three 10 m² areas, as above) |
| Each additional 100 m² (1000 ft²) or part | 5 more (one more 10 m² area) |
Each spot measurement is not a single reading, but the average of at least 3 readings taken within a ~1.5 inch diameter area. This design uses local repeated measurement to suppress random error and makes the spot average more reliable.
Core 2: the acceptance rule (Level 3 by default)
SSPC-PA 2 does not use the 80/20 rule (that belongs to ISO 19840). It sets restriction levels; at Level 3, the default, these conditions apply:
- Each spot measurement (the average of at least 3 gauge readings) ≥ 80 % of the specified minimum and ≤ 120 % of the specified maximum;
- Each area measurement (the average of 5 spots) falls within the specified minimum–maximum range;
- Individual gauge readings are not restricted at Level 3; they are averaged into the spot.
If either limit is not met, the area is judged non-conforming. Projects to ISO 19840 use the 80/20 rule instead — see the“80/20 Rule”article in this section for a worked example.
The appendices: referenced selectively by contract
| Annex | Content |
|---|---|
| Annex 1 | Examples of average thickness measurement and determination of non-conforming area size |
| Annex 2 | Thickness measurement of steel girders |
| Annex 3 | Measurement after shop painting of steel girders, structural steel and miscellaneous items |
| Annex 4 | Measurement method for coating test plates |
| Annex 5 | Measurement of thin coatings after abrasive blasting |
| Annex 6 | Edge coating thickness measurement |
| Annex 7 | Thickness measurement of coated steel pipe exterior |
| Annex 8 | Example of Type 2 instrument shim adjustment |
| Annex 9 | Notes on coating failure investigation |
| Annex 10 | Type 2 instrument continuous scan / scanning probe technique |
| Annex 11 | Thickness measurement of intumescent fireproofing and cryogenic spill protection coatings on structural steel, fire divisions, pipework and vessels/tanks |
Applicable instruments
PA 2 references the D7091 instrument classification in its clauses: Type 1 magnetic pull-off and Type 2 electronic. Current engineering practice is dominated by Type 2; all Dongru coating thickness gauges belong to this class.
Corresponding models in the Dongru product line
The common nominal thickness range for steel anti-corrosion determines model selection: for conventional coating (~100-400 μm) use DR280A (0-1250 μm, dual mode) or DR360A (0-2000 μm); for heavy anti-corrosion and thick coatings use DR380A (0-2000 μm) or DR6000A (0-6000 μm).
Common misconceptions
- ❌ “PA 2 only applies to US projects” — European projects commonly use ISO 19840, whose sampling plan and 80/20 rule differ from PA 2’s spot-and-area limits; for cross-region work follow the contract designation.
- ❌ “Annexes can be ignored” — once referenced by contract they are mandatory, especially Annex 7 (pipe) which is frequently referenced directly in pipeline work.
- ❌ “More spots means a looser judgment” — the acceptance rule does not change; adding spots only makes the assessment reflect the actual distribution more strictly.
Related instruments: DONGRU DR-A5 Automotive Paint Thickness Gauge · DONGRU DR9000A Fire-Resistant Coating Thickness Gauge · Request a quote